Flaking and peeling

Wady lakiernicze - łuszczenie

Occurrence

Lack of adhesion of the coating to the substrate or of individual coats to each other (poor inter-coat adhesion).

Causes

  • Insufficient cleaning of the substrate from silicone, oil, wax, rust, etc.

  • Inadequate surface preparation
  • Use of the wrong primer
  • Primer and/or topcoat too thin
  • Coating too thick
  • Inter-coat drying time too short

Prevention

  • Thoroughly clean and prepare the surface before painting

  • Use well-matched primers
  • Observe the product application parameters specified in the technical data sheets.
  • Apply coatings of sufficient thickness

Removal

Remove the coating from an area slightly larger than the one with the defect. Recoat.