Occurrence

Scratches visible singly or in large numbers on the paint surface which look like sanding lines.

Causes

  • Sanding with too coarse abrasives 
  • Insufficient curing of the filler
  • Insufficiently sanded polyester putty
  • Insufficient insulation of the putty prior to topcoat application

Prevention

  • Use paper of the recommended gradation
  • Isolate the filled areas with filler primer
  • Cure the primer well
  • Use drying times recommended by the manufacturer

Removal

Sand down and reapply both primer and topcoat.