Runs & Sags

Wady lakiernicze - zacieki

Occurrence

Excessive amount of paint that runs down the panel.

Causes

  • Inappropriate choice of paint materials for the application conditions (thinners too slow)

  • Too low paint viscosity
  • Paint or object too cold
  • Too thick coat
  • Drying time too short
  • Gun held too close to the surface or moved too slow
  • Gun nozzle diameter too large

Prevention

  • Use the correct materials in accordance with the manufacturer's recommended technology

Removal

Small sags can be removed by sanding with P1000-P1200 paper and polishing with polishing paste. If there are large patches, the entire coatings should be removed and reapplied