Occurrence

Insufficient coverage - the substrate is visible through the topcoat layer.

Causes

  • Insufficient mixing of topcoat before spraying

  • Topcoat layer sprayed too thin

  • The varnish used has uneven pigmentation

  • Adding too much or using wrong thinner 

Prevention

  • Spray a neutral primer
  • Observe the recommended layer thickness
  • Avoid using too much thinner
  • Mix the varnish thoroughly before application

Removal

Sand with P800/P1000 sandpaper after drying and re-paint.